does anyone have any experience with PC on fenders or other plastics?http://www.pcimag.com/articles/96285-new-technology-enables-powder-coating-for-plastics--composites-and-other-nonmetallic-substratesa project at work brought this to my attention and it might have a place in the ATV world.thanks,john
The article says cure temperatures are in the 250 to 400 deg range. Has anyone tested the OEM plastic to see if it will maintain its shape at those temperatures? It would probably be a good idea to "cook" some OEM plastic for a few hours at a little less than 400 deg to see if the some of the oil/plastic components evaporate from the plastic making it weak or brittle after it returns to room temperature.